Does anyone have any tips or procedures for acid porting heads and intakes? I have always been curious about this.


gahainsey
Member
posted March 23, 2004 06:46 AM
I would at least like to know what kind of acid to use.


KPLugnut
Member
posted March 23, 2004 07:21 AM
That depends on what type of material you're working on. Muriatic acid for aluminum, and sulfuric acid for iron is common.
And remember, the acid is only used to "erase" signs of traditional porting work.

KP

gahainsey
Member
posted March 23, 2004 12:32 PM
Thanks for the input. Maybe I'll run some experiments some day.